厚向强度分布对特厚板三辊预弯成形的影响

仉志强, 付建华, 宋建丽, 金坤善, 李永堂   

  1. 太原科技大学 材料科学与工程学院,太原 030024
  • 收稿日期:2013-09-02 出版日期:2015-05-01 发布日期:2015-05-01
  • 作者简介:仉志强(1982-),男,博士研究生.研究方向:塑性成形工艺与装备.
  • 基金资助:
    山西省重大科技专项项目(20111101032); 山西省高等学校科技创新项目(2015171); 太原科技大学博士启动基金项目(20142040); 太原科技大学青年基金项目(20143010)

Influence of material strength distribution along thickness on three-roller edge pre-bending of thick plate

ZHANG Zhi-qiang, FU Jian-hua, SONG Jian-li, JIN Kun-shan, LI Yong-tang   

  1. School of Material Science and Engineering,Taiyuan University of Science and Technology,Taiyuan 030024,China
  • Received:2013-09-02 Online:2015-05-01 Published:2015-05-01

摘要: 选取100、220 mm两种厚度Q235热轧板,在厚向多个等间距分布位置切取圆棒试样,采用WAW-E100试验机获得各试样在3.0×10-5 s-1应变速率时的拉伸应力应变曲线。根据拉伸试验数据建立考虑厚向强度分布的材料应力-应变函数。分析特厚板在CDW11XNC-300\420 mm×2500 mm重型三辊卷板机上的预弯成形过程并建立预弯工艺模型。预弯模型计算结果表明,特厚板厚向强度变幅为0~20%时,上辊垂直力增幅约为0~13%,回弹比略有增加,卸载前预弯角无明显变化。

关键词: 材料合成与加工工艺, 三辊预弯, 厚向材料强度, 拉伸试验, 特厚板

Abstract: Three-roller edge pre-bending of thick plate is affected by non-uniform material strength distribution along the thickness introduced by multi-pass roll forming and heat treatment. Hot-rolled Q235 plates with thickness of 100 mm and 200 mm were investigated by tensile testing of round bars from equal spaced multi-positions along the thickness. The material stress-strain curves of tensile bars were achieved by tensile testing on WAW-E100 machine at a strain rate of 3.0 × 10-5 s-1. The stress-strain relationship of the material considering the non-uniform distribution was obtained. Three-roller edge pre-bending process of thick plate on CCDW11XNC-300\420×2500 mm heavy machine with bottom rollers horizontally adjustable was analyzed and an edge pre-bending model was developed. Numerical results by this model show that a strength variation of 0~20% along thickness could result in top-roller force variation of 0~13%, little increase in springback ratio, and no effect on pre-bending angle before unloading.

Key words: materials synthesis and processing technology, three-roller edge pre-bending, material strength over thickness, tensile test, thick plate

中图分类号: 

  • TG315.7
[1] Hoggan E J, Scott R I, Barnett M R, et al. Mechanical properties of tension leveled and skin passed steels[J]. Journal of Materials Processing Technology,2002,125-126:155-163.
[2] Weiss M, Rolfe B, Peter D H, et al. Effect of residual stress on the bending of aluminium[J]. Journal of Materials Processing Technology,2012,212(4):877-883.
[3] Fujii K, Ishikawa S, Nakamo Y. Materials properties and residual stresses of rolled thick plate and their effect on static strength[J]. Doboku Gakkai Ronbunshuu A,2010,66(2):253-263.
[4] Hansen N E, Jannerup O. Modeling of elastic-plastic bending of beams using a roller bending machine[J]. J Eng Ind,1979,101(3):304-310.
[5] Shin J G, Park T J, Yim H. Kinematics based determination of three rolling region in roll bending for smoothly curved plates[J]. J Manuf Sci Eng,2001,123(2):284-290.
[6] Gandhi A H, Raval H K. Analytical and empirical modeling of top roller position for three-roller cylindrical bending of plates and its experimental verification[J]. Journal of Materials Processing Technology,2008,197(1):268-278.
[7] Hua M, Lin Y H. Effect of strain hardening on the continuous four-roll plate edge bending process[J]. Journal of Materials Processing Technology,1999,89(1-3):12-18.
[8] 胡卫龙. 板材弯卷变形的理论分析与实验研究[D]. 哈尔滨:哈尔滨工业大学机电工程学院,1992.
Hu Wei-long. The theoretical analysis and experimental study of the plate roll bending[D]. Harbin: School of Mechatronics Engineering,Harbin Institute of Technology,1992.
[9] Wang C T,Kinzel G,Altan T. Mathematical modeling of plane-strain bending of sheet and plate[J]. Journal of Materials Processing Technology,1993,39(3-4):279-304.
[1] 姜秋月,杨海峰,檀财旺. 22MnB5超高强钢焊接接头强化性能[J]. 吉林大学学报(工学版), 2018, 48(6): 1806-1810.
[2] 胡志清, 颜庭旭, 李洪杰, 吕振华, 廖伟, 刘庚. 深冷处理对铝合金薄板冲剪成形性能的影响[J]. 吉林大学学报(工学版), 2018, 48(5): 1524-1530.
[3] 邱小明, 王银雪, 姚汉伟, 房雪晴, 邢飞. 基于灰色关联的DP1180/DP590异质点焊接头工艺参数优化[J]. 吉林大学学报(工学版), 2018, 48(4): 1147-1152.
[4] 陈俊甫, 管志平, 杨昌海, 牛晓玲, 姜振涛, 宋玉泉. 金属棒试样拉伸和扭转试验应变范围和力学特性对比[J]. 吉林大学学报(工学版), 2018, 48(4): 1153-1160.
[5] 梁晓波, 蔡中义, 高鹏飞. 夹芯复合板柱面成形的数值模拟及试验[J]. 吉林大学学报(工学版), 2018, 48(3): 828-834.
[6] 刘子武, 李剑峰. 叶片材料FV520B再制造熔覆层冲蚀损伤行为及评价[J]. 吉林大学学报(工学版), 2018, 48(3): 835-844.
[7] 刘纯国, 刘伟东, 邓玉山. 多点冲头主动加载路径对薄板拉形的影响[J]. 吉林大学学报(工学版), 2018, 48(1): 221-228.
[8] 张志强, 刘从豪, 何东野, 李湘吉, 李纪萱. 基于性能梯度分布的硼钢热冲压工艺对形状精度的影响[J]. 吉林大学学报(工学版), 2017, 47(6): 1829-1833.
[9] 吕萌萌, 谷诤巍, 徐虹, 李欣. 超高强度防撞梁热冲压成形工艺优化[J]. 吉林大学学报(工学版), 2017, 47(6): 1834-1841.
[10] 王辉, 周杰, 熊煜, 陶亚平, 向荣. 基于逆向工程的复杂曲面冲压件回弹补偿[J]. 吉林大学学报(工学版), 2017, 47(6): 1842-1847.
[11] 王春生, 邹丽, 杨鑫华. 基于邻域粗糙集的铝合金焊接接头疲劳寿命影响因素分析[J]. 吉林大学学报(工学版), 2017, 47(6): 1848-1853.
[12] 邢海燕, 葛桦, 李思岐, 杨文光, 孙晓军. 基于模糊隶属度最大似然估计的焊缝隐性缺陷磁记忆信号识别[J]. 吉林大学学报(工学版), 2017, 47(6): 1854-1860.
[13] 谷晓燕, 刘亚俊, 孙大千, 徐锋, 孟令山, 高帅. S355钢/6005A铝合金瞬间液相扩散连接接头组织与性能[J]. 吉林大学学报(工学版), 2017, 47(5): 1534-1541.
[14] 谷诤巍, 张文学, 吕萌萌, 王伟, 徐虹, 李欣. 宽翼边U型截面不锈钢型材拉弯成形缺陷控制[J]. 吉林大学学报(工学版), 2017, 47(4): 1165-1170.
[15] 寇淑清, 宋玮峰, 石舟. 36MnVS4连杆裂解加工模拟及缺陷分析[J]. 吉林大学学报(工学版), 2017, 47(3): 861-868.
Viewed
Full text


Abstract

Cited

  Shared   
  Discussed   
No Suggested Reading articles found!